Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 103 - 138 MPa | 15000 - 20000 psi | Average value: 121 MPa Grade Count:5 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Injection Pressure | 103 - 138 MPa | 14900 - 20000 psi | |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |