Polymer Property : Injection Pressure = 100 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 100 - 150 MPa
14500 - 21800 psi
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne
Injection Pressure 100 - 150 MPa
14500 - 21800 psi
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre
FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Injection Pressure 100 - 140 MPa
14500 - 20300 psi
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Injection Pressure 100 MPa
14500 psi
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Injection Pressure 100 - 140 MPa
14500 - 20300 psi
Plastcom SLOVALEN PH 49 GF 60 PP reinforced with 60% glass fibre
Features: Modified homopolymer PP for injection moulding, chemically reinforced with 60% glass fibre, contains the modifier of mechanical properties.Very good strength and tensile modulus. Delivered..