Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Ejection Temperature 185 °C
365 °F
Covestro Apec® DP 1-9379 Polycarbonate  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha..