Polymer Property : Ejection Temperature = 288 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Ejection Temperature 142 °C
288 °F
Covestro Apec® 1600 Polycarbonate  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay..