Processing Properties | Metric | English | Comments |
---|---|---|---|
Ejection Temperature | 138 °C | 280 °F | |
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Ejection Temperature | 138 °C | 280 °F | |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |