Polymer Property : Ejection Temperature = 152 °C
Polymer Property :
Ejection Temperature =
152 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Ejection Temperature
152
°C
306
°F
Covestro Apec® 1703 Polycarbonate
UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content