Polymer Property : Dry Time = 8 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 8 hour

@Temperature 65.0 - 70.0 °C
8 hour

@Temperature 149 - 158 °F
Maximum
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 82.0 - 87.0 °C
8 hour

@Temperature 180 - 189 °F
Maximum
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 95.0 - 100 °C
8 hour

@Temperature 203 - 212 °F
Maximum
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 95.0 - 100 °C
8 hour

@Temperature 203 - 212 °F
Maximum
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time <= 8 hour

@Temperature 85.0 - 90.0 °C
<= 8 hour

@Temperature 185 - 194 °F
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 87.0 - 95.0 °C
8 hour

@Temperature 189 - 203 °F
Maximum
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 95.0 - 100 °C
8 hour

@Temperature 203 - 212 °F
Maximum
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 85.0 - 90.0 °C
8 hour

@Temperature 185 - 194 °F
Maximum
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Dry Time 8 hour

@Temperature 87.0 - 95.0 °C
8 hour

@Temperature 189 - 203 °F
Maximum
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..