Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 5 - 7 hour @Temperature 150 - 160 °C |
5 - 7 hour @Temperature 302 - 320 °F |
Typical |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |