Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3 - 4 hour @Temperature 82.0 - 87.0 °C |
3 - 4 hour @Temperature 180 - 189 °F |
Typical |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Dry Time | 3 - 4 hour @Temperature 95.0 - 100 °C |
3 - 4 hour @Temperature 203 - 212 °F |
Typical |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Dry Time | 3 - 4 hour @Temperature 95.0 - 100 °C |
3 - 4 hour @Temperature 203 - 212 °F |
Typical |
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Dry Time | 3 - 4 hour @Temperature 87.0 - 95.0 °C |
3 - 4 hour @Temperature 189 - 203 °F |
Typical |
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Dry Time | 3 - 4 hour @Temperature 95.0 - 100 °C |
3 - 4 hour @Temperature 203 - 212 °F |
Typical |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Dry Time | 3 - 4 hour @Temperature 87.0 - 95.0 °C |
3 - 4 hour @Temperature 189 - 203 °F |
Typical |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |