Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 24.0 hour @Temperature 150 - 160 °C |
24.0 hour @Temperature 302 - 320 °F |
Maximum |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Dry Time | 24.0 hour @Temperature 24.0 °C |
24.0 hour @Temperature 75.2 °F |
Full Dry |
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Dry Time | 24.0 hour @Temperature 24.0 °C |
24.0 hour @Temperature 75.2 °F |
Full Dry |
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |