Dry Time 10 - 20.0 hour

@Temperature 24.0 °C
10 - 20.0 hour

@Temperature 75.2 °F
then 30 minutes at 65°C
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding
Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding..