Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 98.9 °C | 210 °F | Optimum cure is 2 hr. @ 210°F |
Armstrong A-40 Epoxy Adhesive Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re.. |