Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 87.8 °C | 190 °F | Mold and Set Temperature |
Spartech Polypedic C Polypropylene Copolymer Description: Resilient in cold weather, durable, slightly less rigid than Polypedic OApplications: AFOs; MAFOs; KAFOs; AK and BK sockets; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; Info.. |
|||
Processing Temperature | 87.8 °C | 190 °F | Mold and Set Temperature |
Spartech Polypedic O Polypropylene Homopolymer Description: Rigid, strong, fatigue-resistantApplications: AFOs; MAFOs; KAFOs; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; AK and BK socketsInformation provided by Spartech. |