Processing Properties Metric English Comments
Processing Temperature 460 °C
860 °F
Typical Firing Temperature; Typical Firing Time: 60 min.
Ferro CF 7575 Display Device
Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for herm..