Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | >= 82.0 °C | >= 180 °F | Immersion |
Henkel Turco C NVT Cleaner Turco C NVT is a heavy-duty, alkaline cleaner for immersion and barrel cleaning operations. It is particularly suited to plating, porcelain enameling and other critical finishing operations which re.. |