Processing Properties Metric English Comments
Processing Temperature 81.0 °C
178 °F
Seal initiation temperature
Dow AFFINITY™ PF 1140 Polyolefin Plastomer
AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre..