Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 670 °C | 1240 °F | Typical Firing Temperature; Typical Firing Time: 5-10 min. |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |