Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 575 °C | 1070 °F | Typical Firing Temperature |
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |