Polymer Property : Processing Temperature = 55.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature >= 55.0 °C
>= 131 °F
Activation Temperature
Lubrizol Advanced Materials Pearlstick® 45-50/03 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/03 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Processing Temperature >= 55.0 °C
>= 131 °F
Activation Temperature
Lubrizol Advanced Materials Pearlstick® 45-50/05 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/05 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Processing Temperature >= 55.0 °C
>= 131 °F
Activation Temperature
Lubrizol Advanced Materials Pearlstick® 45-50/08 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/08 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Processing Temperature 55.0 - 70.0 °C
131 - 158 °F
Immersion
Henkel Turco 6849 Cleaner
Turco 6849 is a clear, aqueous alkaline degreaser formulated to remove shop soils, marking inks, COSMOLINE, grease and lube oils from ferrous and non-ferrous alloys. Offers both exceptional effectiv..
Processing Temperature 55.0 °C
131 °F
humidified air drying temperature
Borealis FR4830 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4830 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4830 is intended for use as a 125º C rated primary ..
Processing Temperature 55.0 °C
131 °F
humidified air drying temperature;2-8h
Borealis FR4837 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4837 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4837 is intended for use as a 125º C rated primary..
Processing Temperature 55.0 °C
131 °F
drying;2-8h
Borealis FR4847 Polyethylene Based Striping Compound
FR4847 is a Polyethylene Based Striping Compound for Primary Automotive Wires. FR4847 is designed and manufactured with advanced material and processing technology to provide enhanced stabilization..
Processing Temperature 55.0 °C
131 °F
humidified air drying temperature;2-8h
Borealis FR4832 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4832 is a Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires. Applications: FR4832 is intended for use as a 125º C rated primary insulation for crosslinked automotive wi..
Processing Temperature 55.0 °C
131 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-50/18 Polycaprolactone based TPU
Pearlstick 45-50/18 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium-low thermoplasticity level. S..
Processing Temperature 55.0 °C
131 °F
Min. Activation Temp; EN 12961
Lubrizol Advanced Materials Pearlstick® 45-50/22 Polycaprolactone based TPU
Pearlstick 45-50/22 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium-low thermoplasticity levelSolu..
Processing Temperature >= 55.0 °C
>= 131 °F
Activation Temperature; EN-12961
Lubrizol Advanced Materials Pearlstick® 45-50/29 Linear Thermoplastic Polyurethane Elastomer
Pearlstick 45-50/29 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..