Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 4.00 - 53.0 °C | 39.2 - 127 °F | Surface temperature |
BASF Master Builders Solutions ChemRex® CX-941 Polyurethane Adhesive CX-941 is a one-component polyurethane-based trowelable-grade structural adhesive. Its patented formula is VOC compliant and contains no chlorinated solvents or water. CX-941 provides excellent in.. |