Polymer Property : Processing Temperature = 331 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 120 - 166 °C
248 - 331 °F
Mold temperature
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert..