Polymer Property : Processing Temperature = 1958 °F
Polymer Property :
Processing Temperature =
1958 °F
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Processing Temperature
1070
°C
1958
°F
Flow Temp
Wieland Porta IP V-1 Solder
Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental