Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1070 °C | 1950 °F | fusing temperature |
Wall Colmonoy COLMONOY® 6 PTA Nickel-Base Hard Surfacing Alloy With Chromium Boride Description: Optimized formulation to offset dilution and alloy loss from the arc. Designed for PTA Application.Applications: Colmonoy 6 PTA is designed for plasma transferred arc (PTA) application... |
|||
Processing Temperature | 1070 °C | 1950 °F | fusing temperature |
Wall Colmonoy COLMONOY® 52 SA - Hard Nickel-Chromium-Boron Alloy Containing Chromium Carbides Description and Application: Similar to Colmonoy No. 62 SA, but has increased ductility with almost the same abrasion and corrosion resistance. Finished by grinding.Method of Application: Sprayweld.. |
|||
Processing Temperature | 1070 °C | 1950 °F | fusing temperature |
Wall Colmonoy COLMONOY® 23A & 24 - Nickel Alloy With Tungsten Carbide Description and Application: Used to repair blow holes, flaws, chips, and cracks in cast iron parts. No. 23A works best in repairing surface flaws, No. 24 is recommended for working on edges or cor.. |