Polymer Property : Processing Temperature = 1620 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 880 °C
1620 °F
Typical Firing Temperature; Typical Firing Time: 10-20 min. at Peak
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..
Processing Temperature 882 °C
1620 °F
Flow Temp
Wieland Porta Optimum 880 Solder
Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental