Polymer Property : Processing Temperature = 1345 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 729.4 - 851.7 °C
1345 - 1565 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy
Silvaloy A34T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult wet metals su..