Processing Properties Metric English Comments
Processing Temperature 1090 °C
1994 °F
Flow Temp
Wieland Porta 1090-W Solder
Solder supplied as strip (0.18 oz. roll)Information provided by WielandDental
Processing Temperature 1090 °C
2000 °F
fusing temperature
Wall Colmonoy COLMONOY® 5 PTA - Nickel-Base Hard Surfacing Alloy With Chromium Boride
Description: Optimized Colmonoy 5 formulation. Designed for PTA Application.Applications: For plasma transferred arc (PTA) application.Information provided by Wall Colmonoy Corporation.
Processing Temperature 1090 °C
2000 °F
fusing temperature
Wall Colmonoy WALLEX 50 - Cobalt-Nickel Alloy
Description: Good corrosion resistance and low coefficient-of-friction provides good metal-to-metal wear protection (not involving much impact). For bushings, knives and cams. Finished by grinding..
Processing Temperature 1090 °C
2000 °F
fusing temperature
Wall Colmonoy COLMONOY® 84 Nickel-Based Alternative to Cobalt Surfacing Alloys
Description and Application: A nickel-based alternative to cobalt surfacing alloys, for service temperatures up to 1500°F. Boron and silicon content provide better weldability at lower application..