Polymer Property : Processing Temperature = 1080 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 580 °C
1080 °F
Typical Firing Temperature; Typical Firing Time: 10 min.
Ferro EG 4010 Display Device
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas..
Processing Temperature 582 - 604 °C
1080 - 1120 °F
Brazing Range
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought..