Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1030 °C | 1890 °F | fusing temperature |
Wall Colmonoy COLMONOY® 6 Nickel-Base Hard-Surfacing Alloy With Chromium Boride Description: The original, nickel-base hard-surfacing alloy, containing diamond-like chromium borides (and carbides). Extremely resistant to wear, especially under corrosive conditions. Low coeffi.. |
|||
Processing Temperature | 1030 °C | 1890 °F | fusing temperature |
Wall Colmonoy COLMONOY® 69 SC - Alloy With Chromium Carbide Description and Application: Enhanced Colmonoy 69, with more chromium and molybdenum for better corrosion resistance. Improved plastic range makes overlays easier to fuse without sagging. For mari.. |
|||
Processing Temperature | 1030 °C | 1880 °F | fusing temperature |
Wall Colmonoy COLMONOY® 5 - Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides Description: Contains wear-resistant chromium borides and carbides. Has greater ductility, better impact resistance and workability than Colmonoy No. 6 Finished with carbide tools and grinding.App.. |