Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1000 °C | 1830 °F | Typical Firing Temperature |
Ferro EG 1001 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Gun Mount Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for.. |
|||
Processing Temperature | >= 1000 °C | >= 1830 °F | Typical Firing Temperature |
Ferro EG 2770 Specialty Glass Glass Type: Si-Al-Mg-Ca Typical Powder Form: TF Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Processing Temperature | 1000 °C | 1830 °F | Typical Firing Temperature |
Ferro EG 2790 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,.. |
|||
Processing Temperature | 1000 °C | 1832 °F | Cuvette Temp |
Wieland 1945 Wilaform Platinum Platinum alloy for universal use.Applications: chains, coin/shape, laminar decoration, pipes, tubingDental |
|||
Processing Temperature | 1000 °C | 1832 °F | Cuvette Temp |
Wieland 1951 Wilaform Platinum Platinum alloy for technical use.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Processing Temperature | 1000 °C | 1830 °F | Typical Firing Temperature |
Ferro EG 2800 Metal Sealing Glass Type: CA-Si-B Typical Powder Form: VSD Typical Application: TA 23 Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |