Polymer Property : Specific Heat Capacity = 3.02 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 3.02 J/g-°C

@Temperature 288 °C
0.721 BTU/lb-°F

@Temperature 550 °F
Duratherm LT Paraffinic Heat Transfer Fluid
Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat..