Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.13 J/g-°C @Temperature 37.8 °C |
0.510 BTU/lb-°F @Temperature 100 °F |
|
Duratherm 450 Paraffinic Heat Transfer Fluid Duratherm 450 - thermal fluid specifically engineered for applications requiring process heating and cooling efficiently between 30°F and 450°F. Economical and thermally stable, Duratherm 450 offe.. |
|||
Specific Heat Capacity | 2.13 J/g-°C @Temperature 100 °C |
0.509 BTU/lb-°F @Temperature 212 °F |
|
Dow VORANOL™ 4703 Polyether Polyol VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resil.. |