Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.39 J/g-°C @Temperature 50.0 °C |
0.332 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Specific Heat Capacity | 1.39 J/g-°C @Pressure 20.3 MPa, Temperature 24.0 °C |
0.332 BTU/lb-°F @Pressure 2940 psi, Temperature 75.2 °F |
|
3M Interam™ E-5A-4 Endothermic Mat When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap.. |
|||
Specific Heat Capacity | 1.39 J/g-°C @Temperature 50.0 °C |
0.332 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |