Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.15 J/g-°C @Temperature 500 °C |
0.275 BTU/lb-°F @Temperature 932 °F |
|
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance .. |