Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.13 J/g-°C @Temperature 50.0 °C |
0.270 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Specific Heat Capacity | 1.13 J/g-°C @Temperature 50.0 °C |
0.270 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |