Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.975 J/g-°C @Temperature 580.0 °C |
0.233 BTU/lb-°F @Temperature 1076 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |