Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.761 J/g-°C @Temperature 17.9 °C |
0.182 BTU/lb-°F @Temperature 64.1 °F |
|
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |