Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |