Thermal Properties Metric English Comments
Specific Heat Capacity 0.569 J/g-°C

@Temperature 400 °C
0.136 BTU/lb-°F

@Temperature 752 °F
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..