Polymer Property : Specific Heat Capacity = 0.536 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 600 °C
0.128 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.536 J/g-°C

@Temperature 299 °C
0.128 BTU/lb-°F

@Temperature 570 °F
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha..