Thermal Properties Metric English Comments
Specific Heat Capacity 2.18 J/g-°C

@Temperature 240 °C
0.521 BTU/lb-°F

@Temperature 464 °F
Eastman Eastar AN004 Natural PCTA Copolyester
EASTAR AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exp..