Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.520 J/g-°C @Temperature 300 °C |
0.124 BTU/lb-°F @Temperature 572 °F |
|
International Mold Steel Daido DRM3 Matrix High-Speed Steel This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio.. |
|||
Specific Heat Capacity | 0.520 J/g-°C @Temperature 260 °C |
0.124 BTU/lb-°F @Temperature 500 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |