Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 400 °C |
0.112 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.468 J/g-°C @Temperature 100 °C |
0.112 BTU/lb-°F @Temperature 212 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |