Thermal Properties Metric English Comments
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 23.0 °C
0.109 BTU/lb-°F

@Temperature 73.4 °F
Special Metals INCONEL® alloy 693
INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t..
Specific Heat Capacity 0.455 J/g-°C

@Temperature 300 °C
0.109 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..