Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Specific Heat Capacity | 0.434 J/g-°C @Temperature 100 °C |
0.104 BTU/lb-°F @Temperature 212 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |