Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.69 J/g-°C @Temperature 37.8 °C |
0.403 BTU/lb-°F @Temperature 100 °F |
|
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |