Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.59 J/g-°C @Temperature -73.3 °C |
0.380 BTU/lb-°F @Temperature -100 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |