Thermal Properties Metric English Comments
Specific Heat Capacity 0.700 J/g-°C

@Temperature 100 - 200 °C
0.167 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 20.0 °C
0.167 BTU/lb-°F

@Temperature 68.0 °F
DINV ENV 821-3
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 25.0 °C
0.167 BTU/lb-°F

@Temperature 77.0 °F
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber
Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance ..
Specific Heat Capacity 0.700 J/g-°C

@Temperature 538 °C
0.167 BTU/lb-°F

@Temperature 1000 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..