Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.695 J/g-°C @Temperature 550.0 °C |
0.166 BTU/lb-°F @Temperature 1022 °F |
|
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |
|||
Specific Heat Capacity | 0.694 J/g-°C @Temperature 500 °C |
0.166 BTU/lb-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |