Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.628 J/g-°C @Temperature 400 °C |
0.150 BTU/lb-°F @Temperature 752 °F |
|
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type) PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3.. |
|||
Specific Heat Capacity | 0.626 J/g-°C @Temperature 1000 °C |
0.150 BTU/lb-°F @Temperature 1830 °F |
|
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |
|||
Specific Heat Capacity | 0.627 J/g-°C @Temperature 700 °C |
0.150 BTU/lb-°F @Temperature 1290 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |