Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.554 J/g-°C @Temperature 400 °C |
0.132 BTU/lb-°F @Temperature 752 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |